Support rod

Product Description:

The carbon/carbon support rod is a core structural component of the thermal system in photovoltaic single-crystal silicon growth furnaces, providing stable support for the quartz crucible and molten silicon at ultra-high temperatures ranging from 1600 to 2200°C. Additionally, it enables optimized directional heat transfer, helping to fine-tune the temperature gradient at the crystal growth interface.

 

Recommended grades:

KBC-13B

Density, g/cm³:

≥1.30

Flexural strength, MPa:

≥110

Compressive strength, MPa:

≥160

Room-temperature thermal conductivity, W/(m·K):

≤10

Keywords:

Related Products

Crucible


Recommended grades:

KBC-14A

Density, g/cm³:

≥1.40

Flexural strength, MPa:

≥120

Compressive strength, MPa:

≥150

Room-temperature thermal conductivity, W/(m·K):

≥20

Insulation Cylinder


Recommended grades:

KBC-11

Density, g/cm³:

≥1.10

Flexural strength, MPa:

≥80

Coefficient of thermal expansion, 10 -6 /K

≤1.0

Room-temperature thermal conductivity, W/(m·K):

≤10

Outer Guide Tube


Recommended grades:

KBC-13A

Density, g/cm³:

≥1.35

Flexural strength, MPa:

≥110

Coefficient of thermal expansion, 10 -6 /K

≤1.0

Room-temperature thermal conductivity, W/(m·K):

≤10

Internal Guide Tube


Recommended grades:

KBC-13A

Density, g/cm³:

≥1.35

Flexural strength, MPa:

≥110

Coefficient of thermal expansion, 10 -6 /K

≤1.0

Room-temperature thermal conductivity, W/(m·K):

≤10

Crucible holder


Recommended grades:

KBC-13B

Density, g/cm³:

≥1.30

Flexural strength, MPa:

≥110

Compressive strength, MPa:

≥160

Coefficient of thermal expansion, 10 -6 /K

≤1.0

Supporting Ring


Recommended grades:

KBC-12A

Density, g/cm³:

≥1.20

Flexural strength, MPa:

≥110

Compressive strength, MPa:

≥120

Coefficient of thermal expansion, 10 -6 /K

≤1.0